Arkema Group Lacovyl® PB 8050 PVC

Category Polymer , Thermoplastic , Vinyl (PVC) , PVC, Molded
Manufacturer Arkema
Trade Name Lacovyl®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Arkema Group Lacovyl® PB 8050 PVC.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LACOVYL PB 8050 is a vinyl chloride homopolymer obtained by the mass polymerization process. It can be incorporated with plastisol based on microsuspension - or emulsion - polymerized PVC to : obtain a lower-cost formulation, reduce and stabilize viscosity in storage, enhance pseudo-plasticity, reduce gloss in surface layers, improve transparency and thermal stability. By virtue of its exceptionally fine state of division, it can be used in the thinnest possible layers.It is usable in every type of application, at up to 50 phr in certain cases.* MAIN PROPERTIES Viscosity index (ISO 1628-2):79 ml/g,(K value:57). * APPLICATIONSLACOVYL PB 8050 can be used in all plastisol applications in the manufacture of materials for the building industry (floor and wall coverings), the motor industry (artificial leather and mastics), the food industry (closures, etc...), morocco-leather goods, footwear (artificial leather), etc. toys, balls, dolls, etc. ISO data provided by the manufacturer, Arkema.
Physical Properties Metric English Comments
Viscosity Test 79 cm³/g
79 cm³/g
Viscosity Number
Optical Properties Metric English Comments
Transmission, Visible 80 %
80 %
Mfr. reports 'Transparent' but doesn't quantify.