Arkema Group Lacovyl® GB 1350 PVC

Category Polymer , Thermoplastic , Vinyl (PVC) , PVC, Transparent
Manufacturer Arkema
Trade Name Lacovyl®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Arkema Group Lacovyl® GB 1350 PVC.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LACOVYL GB 1350 is a vinyl chloride homopolymer produced by mass polymerization process.CHARACTERISTICS Viscosity index (ISO 1628-2):125 ml/g,(K value:70). Apparent density (ISO 60 ):0.55 g/ml. high rate of plasticizer absorption. high molecular weight giving articles with good mechanical properties. very good transparency. RECOMMENDED APPLICATIONS standard and transparent soling. premolded soling. EXAMPLES OF APPLICATIONS, PVC-P: NAKAN FSS 703 R NAKAN FSS 601 R ISO data provided by the manufacturer, Arkema.
Physical Properties Metric English Comments
Apparent Bulk Density 0.540 g/cc
0.0195 lb/in³
Viscosity Test 125 cm³/g
125 cm³/g
Viscosity Number
Optical Properties Metric English Comments
Transmission, Visible 80 %
80 %
Mfr. reports 'Transparent' but doesn't quantify.