Material Notes:
LACOVYL EF 701 is a vinyl chloride homopolymer manufactured by emulsion polymerization process for the preparation of plastisols.* MAIN CHARACTERISTICSViscosity index (ISO 1628-2):125 ml/g,(K value:70).* APPLICATIONSLACOVYL EF 701 may be used in the following areas: compact layer: wall coverings or coated fabrics. foam layer by mechanical or chemical techniques. rotational molding: toys, bumpers, buoys, car parts. dip molding. slush molding. cap closures. ISO data provided by the manufacturer, Arkema.
Physical Properties Metric English Comments
Viscosity Test 125 cm³/g
125 cm³/g
Viscosity Number