Arkema Group LOTADER® 5500 Terpolymer Ethylene - Acrylic Ester - Maleic Anhydride

Category Polymer , Adhesive , Thermoplastic , EMAAA Terpolymer
Manufacturer Arkema
Trade Name LOTADER®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Arkema Group LOTADER® 5500 Terpolymer Ethylene - Acrylic Ester - Maleic Anhydride.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LOTADER 5500 is a random terpolymer of Ethylene, Acrylic Ester and Maleic Anhydride, polymerized by high pressure autoclave process. These grade is characterised by a high fluidity. Functional groups contribute to the outstanding adhesive properties of LOTADER 5500 on various substrates. LOTADER 5500 is mainly used pure or in blends with polyolefins as thermoadhesive films or adhesives.Information provided by Arkema Group
Physical Properties Metric English Comments
Density 0.940 g/cc

@Temperature 23.0 °C
0.0340 lb/in³

@Temperature 73.4 °F
ISO 1183
Melt Index of Compound 20 g/10 min

@Load 2.16 kg,
Temperature 190 °C
20 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore A 93
93
ASTM D2240
Tensile Strength at Break 10.0 MPa
1450 psi
ASTM D638
Elongation at Break 700 %
700 %
ASTM D638
Flexural Modulus 0.0450 GPa
6.53 ksi
ASTM D638
Thermal Properties Metric English Comments
Melting Point 80.0 °C
176 °F
DSC
Vicat Softening Point 45.0 °C

@Load 0.999 kg
113 °F

@Load 2.20 lb
ASTM D1525
Descriptive Properties Value Comments
Ethyl Acrylate Content (%) 20
IRTF (internal)
Maleic Anhydride Content (%) 2.8
IRTF (internal)