Material Notes:
EVA copolymer made by high pressure tubular process. Anti-UV stabilized grade. Applications Grade for transparent and thermal agricultural film to 180 at 200 µ for greenhouse coverage.ISO data provided by the manufacturer, Arkema.
Physical Properties Metric English Comments
Density 0.935 g/cc
0.0338 lb/in³
Melt Flow 0.45 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.45 g/10 min

@Load 4.76 lb,
Temperature 374 °F
Mechanical Properties Metric English Comments
Tensile Strength, Yield 6.00 MPa
870 psi
50 mm/min
Elongation at Break >= 50 %
>= 50 %
Nominal Strain; 50 mm/min
Tensile Modulus 0.0500 GPa
7.25 ksi
1 mm/min
Thermal Properties Metric English Comments
Melting Point 93.0 °C
199 °F
10°C/min
Vicat Softening Point 73.0 °C
163 °F
50°C/hr; 50N
Optical Properties Metric English Comments
Transmission, Visible 80 %
80 %
Mfr. reports 'Transparent' but doesn't quantify.