Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Arkema Group EVATANE® 24-03 Copolymer Ethylene - Vinyl Acetate

Category Polymer , Thermoplastic , Ethylene Vinyl Acetate , Ethylene Vinyl Acetate Copolymer (EVA), Adhesive/Sealant Grade
Manufacturer Arkema
Trade Name Evatane®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Arkema Group EVATANE® 24-03 Copolymer Ethylene - Vinyl Acetate.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
EVATANE® 24-03 is a random copolymer of Ethylene and Vinyl Acetate made by high-pressure radicalar polymerisation process. EVATANE® 24-03 is stabilized with antioxidants. The High Vinyl Acetate content of EVATANE® 24-03 brings softness, flexibility and polarity. EVATANE® 24-03 delivers high cohesive strength with any kind of fillers (masterbatchs, HFFR compounds). EVATANE® 24-03 is also very well adapted for the production of cast or blown films. It can also be used as an additive for bitumen.Information provided by Arkema Group
Physical Properties Metric English Comments
Density 0.940 g/cc

@Temperature 23.0 °C
0.0340 lb/in³

@Temperature 73.4 °F
ISO 1183
Vinyl Acetate Content 23 - 25 %
23 - 25 %
FTIR (internal)
Melt Index of Compound 2.5 - 3.5 g/10 min

@Load 2.16 kg,
Temperature 190 °C
2.5 - 3.5 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore A 83
83
ASTM D2240
Tensile Strength at Break 27.0 MPa
3920 psi
ASTM D638
Elongation at Break 600 - 900 %
600 - 900 %
ASTM D638
Thermal Properties Metric English Comments
Melting Point 80.0 °C
176 °F
DSC
Vicat Softening Point 46.0 °C

@Load 0.999 kg
115 °F

@Load 2.20 lb
ISO 306
Ring & Ball Softening Point 183 °C
361 °F
ASTM E28
Processing Properties Metric English Comments
Processing Temperature <= 230 °C
<= 446 °F