Aremco Pyro-Tape™ 682-HR High Temperature Tape Bi-layer aluminum/fiberglass with silicone adhesive

Category Polymer , Adhesive , Tape
Manufacturer Aremco
Trade Name Pyro-Tape™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Aremco Pyro-Tape™ 682-HR High Temperature Tape Bi-layer aluminum/fiberglass with silicone adhesive.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Applications Heat Reflection Features Protective wrap for pipes exposed to high heat. Heat mask for process instrumentation. Protective wrap for chutes, rails and slides.
Physical Properties Metric English Comments
Thickness 196 microns
7.70 mil
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 260 °C
500 °F
Minimum Service Temperature, Air -73.0 °C
-99.4 °F
Descriptive Properties Value Comments
Adhesion 40 oz/in
Tape Tensile Strength 150 lbs/in