Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Aremco Aremco-Bond™ 556-LV Electrically & Thermally Conductive Material, Silver Filled

Category Polymer , Adhesive , Thermoset , Epoxy
Manufacturer Aremco
Trade Name Aremco-Bond™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Aremco Aremco-Bond™ 556-LV Electrically & Thermally Conductive Material, Silver Filled.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Electrically Conductive, Silver-Filled Epoxy Good Corrosion Resistance and Mechanical Strength to 340 ºF. Paste and Low Viscosity Systems Available.
Physical Properties Metric English Comments
Specific Gravity 2.90 g/cc
2.90 g/cc
mixed, at 25°C
Particle Size <= 20 µm
<= 20 µm
Viscosity 4000 - 6000 cP
4000 - 6000 cP
Mixed Viscosity at 25°C
Mechanical Properties Metric English Comments
Hardness, Shore D 84
84
Shear Strength 7.58 MPa
1100 psi
Tensile Shear
Thermal Properties Metric English Comments
Thermal Conductivity 2.20 W/m-K
15.3 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 171 °C
340 °F
continuous
191 °C
375 °F
intermittent
Electrical Properties Metric English Comments
Volume Resistivity 0.000800 ohm-cm
0.000800 ohm-cm
Processing Properties Metric English Comments
Cure Time 120 min

@Temperature 93.3 °C
2.00 hour

@Temperature 200 °F
Recommended Cure
1440 min

@Temperature 22.2 °C
24.0 hour

@Temperature 72.0 °F
Alternative Cure
Pot Life 60.0 min

@Temperature 25.0 °C
60.0 min

@Temperature 77.0 °F
25 g
Shelf Life 6.00 Month
6.00 Month
Descriptive Properties Value Comments
Color Silver
Filler Silver Flake
Mix Ratio By Weight 100:4
resin:hardener
Copyright © lookpolymers.com All Rights Reserved