Aptek UVIBOND 7100 Semi-rigid, UV-Curing Urethane Adhesive

Category Polymer , Adhesive , Thermoset , Polyurethane, TS , Thermoset Polyurethane, Adhesive
Manufacturer Aptek Laboratories
Trade Name UVIBOND
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Aptek UVIBOND 7100 Semi-rigid, UV-Curing Urethane Adhesive.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
UVIBOND 7100 is an unfilled, one component, electrically insulating, transparent, semi-rigid urethane adhesive designed for bonding polycarbonate, ABS, glass and other various substrates. UVIBOND 7100 is fully curable when exposed to the proper UV radiation.U.V. curable for extremely fast production output; Semi-rigid for high strength bonds with a degree of flexibility; Low viscosity for easy handling and substrate wetting; Low ionic impurities for electrical/electronic applications; Thixotropic version available for doming and staking applications designated as APTEK 97034Information provided by Aptek Laboratories, Inc.
Physical Properties Metric English Comments
Density 1.01 g/cc
0.0365 lb/in³
ASTM D1475
Viscosity 4000 cP
4000 cP
ASTM D1824
Mechanical Properties Metric English Comments
Hardness, Shore A 95
95
Property taken 1 hr after U.V. exposure, 1/16" casting; ASTM D2240
Optical Properties Metric English Comments
Transmission, Visible 90 %
90 %
transparent; thickness not quantified