Applied Composites 8038 Polyester SMC

Category Polymer , Thermoset , Filled/Reinforced Thermoset , Polyester, TS , Thermoset Polyester Glass SMC
Manufacturer Applied Composites Corporation
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Applied Composites 8038 Polyester SMC.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Industry Application: TransportationProduct Application: Mass TransitDistinct Features: Low Smoke Construction and Mass Transit, Oxygen Matex 80+, E84-61 TunnelInformation provided by Applied Composites Corporation.
Physical Properties Metric English Comments
Density 2.01 g/cc
0.0726 lb/in³
ASTM D792
Water Absorption 0.20 %
0.20 %
ASTM D570
Linear Mold Shrinkage 0.0010 cm/cm
0.0010 in/in
Cold Part VS Cold Tool; ASTM D955
Mechanical Properties Metric English Comments
Hardness, Barcol 60
60
ASTM D2583
Tensile Strength, Ultimate 75.8 MPa
11000 psi
ASTM D638
Tensile Modulus 12.4 GPa
1800 ksi
ASTM D638
Flexural Strength 172 MPa
25000 psi
ASTM D790
Flexural Modulus 10.3 GPa
1500 ksi
Tangent; ASTM D790
Compressive Strength 165 MPa
24000 psi
ASTM D695
Izod Impact, Notched 5.34 J/cm
10.0 ft-lb/in
ASTM D256
Taber Abrasion, mg/1000 Cycles 0.40
0.40
% Loss 1000 Cycles; FTMS1091