Material Notes:
Industry Application: TransportationProduct Application: Auto InteriorsInformation provided by Applied Composites Corporation.
Physical Properties Metric English Comments
Density 1.90 g/cc
0.0686 lb/in³
ASTM D792
Water Absorption 0.41 %
0.41 %
ASTM D570
Mechanical Properties Metric English Comments
Hardness, Barcol 65
65
ASTM D2583
Tensile Strength, Ultimate 89.6 MPa
13000 psi
ASTM D638
Flexural Strength 211 MPa
30600 psi
ASTM D790
Flexural Modulus 8.791 GPa
1275 ksi
Secant at 2.5 Deflection; ASTM D790
9.65 GPa
1400 ksi
Secant at 0.5 Deflection; ASTM D790
11.0 GPa
1600 ksi
Tangent; ASTM D790
Compressive Strength 193 MPa
28000 psi
ASTM D695
Izod Impact, Notched 7.47 J/cm
14.0 ft-lb/in
ASTM D256
Izod Impact, Unnotched 9.08 J/cm

@Temperature 23.0 °C
17.0 ft-lb/in

@Temperature 73.4 °F
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) >= 232 °C
>= 450 °F
Flexural Load; ASTM D648