Material Notes:
Synthetic mullite available in rod, tube, sheaths and insulators up to 10 ft (3 m) long with diameters 0.3" to 19".Information provided by Anderman Ceramics.
Physical Properties Metric English Comments
Density 2.70 g/cc
0.0975 lb/in³
Open Porosity 0.00 %
0.00 %
Gas Tight
Mechanical Properties Metric English Comments
Hardness, Mohs 8.0
8.0
Flexural Strength 159 MPa
23000 psi
Thermal Properties Metric English Comments
CTE, linear 5.50 µm/m-°C

@Temperature 20.0 - 1000 °C
3.06 µin/in-°F

@Temperature 68.0 - 1830 °F
Thermal Conductivity 5.00 W/m-K

@Temperature 20.0 - 100 °C
34.7 BTU-in/hr-ft²-°F

@Temperature 68.0 - 212 °F
Maximum Service Temperature, Air 1600 °C
2910 °F
Component Elements Properties Metric English Comments
Al2O3 62 %
62 %
CaO 0.18 %
0.18 %
Fe2O3 0.82 %
0.82 %
SiO2 36 %
36 %
TiO2 0.39 %
0.39 %
Electrical Properties Metric English Comments
Electrical Resistivity 1.00e+13 ohm-cm
1.00e+13 ohm-cm
1.00e+6 ohm-cm

@Temperature 600 °C
1.00e+6 ohm-cm

@Temperature 1110 °F
Dielectric Constant 6.0

@Frequency 1.00e+6 Hz
6.0

@Frequency 1.00e+6 Hz
Descriptive Properties Value Comments
Thermal Shock Resistance Excellent