Anderman Ceramics EC90P Mullite-Bonded Porous Silicon Carbide (90%)

Category Ceramic , Carbide
Manufacturer Anderman Ceramics
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Anderman Ceramics EC90P Mullite-Bonded Porous Silicon Carbide (90%).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Excellent thermal shock properties and thermal conductivity when in contact with molten metal. Available as tube, sheath, or rod up to 6 ft (1.9 m) long with diameters 0.6" to 3.75".Information provided by Anderman Ceramics.
Physical Properties Metric English Comments
Density 2.20 g/cc
0.0795 lb/in³
Open Porosity 25 %
25 %
Thermal Properties Metric English Comments
CTE, linear 5.00 µm/m-°C

@Temperature 20.0 - 1000 °C
2.78 µin/in-°F

@Temperature 68.0 - 1830 °F
Thermal Conductivity 25.0 W/m-K

@Temperature 20.0 - 100 °C
174 BTU-in/hr-ft²-°F

@Temperature 68.0 - 212 °F
Maximum Service Temperature, Air 1450 °C
2640 °F
Component Elements Properties Metric English Comments
Al2O3 6.5 %
6.5 %
SiC 90 %
90 %
SiO2 3.5 %
3.5 %
Descriptive Properties Value Comments
Thermal Shock Resistance Excellent