Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Ametek 17-4 P/M Process, Sintered at 2200°F (1204°C)

Category Metal , Ferrous Metal , Stainless Steel , Precipitation Hardening Stainless
Manufacturer Ametek
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ametek 17-4 P/M Process, Sintered at 2200°F (1204°C).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Composition reported is typical of 17-4 precipitation hardening stainless. This alloy is widely used because of its high strength, high hardness, excellent corrosion resistance, and easy heat treatment. The 17-4 PH alloy is used in aerospace, medical, food processing, and chemical industries for applications such as pump shafts, valve stems, braces, fasteners, coupling, rocket and missile components, hydraulic actuators, and wear rings.Mechanical property data below is from samples aged for 1 hour at 900°F (482°C) in hydrogen - the H900 condition, which maximizes strength. The properties that can be expected for material that was lubricated with 3/4% Acrawax C and compacted at 48 tsi are shown below.17-4 PH is a registered trademark of Armco, Inc.; information provided by Ametek Specialty Metal Product Division.
Mechanical Properties Metric English Comments
Hardness, Rockwell B 100
100
Tensile Strength, Ultimate 860 MPa
125000 psi
Tensile Strength, Yield 610 MPa
88500 psi
Elongation at Break 1.6 %
1.6 %
Component Elements Properties Metric English Comments
Carbon, C 0.035 %
0.035 %
Chromium, Cr 16.3 %
16.3 %
Copper, Cu 4.0 %
4.0 %
Iron, Fe 74 %
74 %
as balance
Manganese, Mn 0.50 %
0.50 %
Nickel, Ni 4.0 %
4.0 %
Niobium, Nb (Columbium, Cb) 0.30 %
0.30 %
Phosphorous, P 0.020 %
0.020 %
Silicon, Si 0.50 %
0.50 %
Sulfur, S 0.015 %
0.015 %
Users viewing this material also viewed the following: