Material Notes:
Product CharacteristicsGood Environmental Stress Crack Resistance (ESCR)Good practical toughnessDeep draw thermoforming capableGood low temperature impactFood Contact CompliantTypical ApplicationsPackaging for foods such as yot, sour cream, delicatessen salads and gravyContainers and lidsCold temperature packagingPortion dairy containersInformation provided by AmericasStyrenics LLC.
Physical Properties Metric English Comments
Specific Gravity 1.04 g/cc
1.04 g/cc
ASTM D792
Linear Mold Shrinkage 0.0040 - 0.0080 cm/cm
0.0040 - 0.0080 in/in
ASTM D955
Melt Flow 3.2 g/10 min

@Load 5.00 kg,
Temperature 200 °C
3.2 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 93
93
ASTM D785
Tensile Strength at Break 21.4 MPa
3100 psi
ASTM D638
Tensile Strength 20.0 MPa
2900 psi
ASTM D638
Elongation at Break 75 %
75 %
ASTM D638
Tensile Modulus 1.45 GPa
210 ksi
ASTM D638
Flexural Strength 28.3 MPa
4100 psi
ASTM D790
Flexural Modulus 1.45 GPa
210 ksi
ASTM D790
Izod Impact, Notched 1.07 J/cm
2.00 ft-lb/in
compression molded; ASTM D256
1.44 J/cm
2.70 ft-lb/in
injection molded; ASTM D256
Thermal Properties Metric English Comments
CTE, linear 90.0 µm/m-°C
50.0 µin/in-°F
ASTM D696
Deflection Temperature at 0.46 MPa (66 psi) 89.4 °C
193 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 79.4 °C
175 °F
ASTM D648
Vicat Softening Point 101 °C
213 °F
ASTM D1525