Material Notes:
API 505 is an intermediate grade of impact modified polystyrene. This material has exceptional moldability and colorability.Applications: API 505 is widely used in housewares, toys, containers, displays and a wide range of injection molded applications.Information provided by American Polymers, Inc.
Physical Properties Metric English Comments
Density 1.04 g/cc
0.0376 lb/in³
ASTM D792
Melt Flow 8.0 g/10 min
8.0 g/10 min
Condition G; ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell L 59
59
ASTM D785
Tensile Strength, Ultimate 29.0 MPa
4200 psi
ASTM D638
Elongation at Break 35 %
35 %
ASTM D638
Tensile Modulus 1.65 GPa
240 ksi
ASTM D638
Flexural Modulus 1.72 GPa
250 ksi
ASTM D790
Izod Impact, Notched 0.694 J/cm

@Thickness 3.17 mm
1.30 ft-lb/in

@Thickness 0.125 in
injection molded sample; ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 85.0 °C
185 °F
Annealed; ASTM D648
Vicat Softening Point 93.9 °C
201 °F
ASTM D1525