American Elements Magnesium Oxide Nanopowder

Category Ceramic , Oxide , Magnesium Oxide
Manufacturer American Elements
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF American Elements Magnesium Oxide Nanopowder.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
General DescriptionMagnesium Oxide Nanoparticles or Magnesia Nanoparticles (MgO) Nanoparticles, nanodots or nanopowder are spinel, high surface area particles. Nanoscale Magnesium Oxide Nanoparticles or Magnesia Particles are typically 5 - 100 nanometers (nm) with specific surface area (SSA) in the 25 – 50 m 2 /g range. Nano Magnesium Oxide Particles are also available in Ultra high purity and high purity and coated and dispersed forms. Applications for magnesium oxide nanocrystals include as an anti-microbial, anti-biotic (biocide) and anti-fungal (fungicide) agent when incorporated in coatings, bandages, nanofiber, nanowire, plastics, alloy and textiles and further research for their potential electrical, optical, imaging, and other biomedical and bioscience properties.
Physical Properties Metric English Comments
Density 3.60 g/cc
0.130 lb/in³
Particle Size 0.0050 - 0.10 µm
0.0050 - 0.10 µm
Specific Surface Area 25 - 50 m²/g
25 - 50 m²/g
Molecular Weight 40.3 g/mol
40.3 g/mol
Thermal Properties Metric English Comments
Melting Point 2830 °C
5130 °F
Boiling Point 3600 °C
6510 °F
Descriptive Properties Value Comments
Appearance Black