American Elements Lutetium Nanoparticles

Category Metal , Nonferrous Metal , Pure Element
Manufacturer American Elements
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF American Elements Lutetium Nanoparticles.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
General DescriptionLutetium (Lu) Nanoparticles, nanodots or nanopowder are black spherical high surface area particles. Nanoscale Lutetium Particles are typically 10 - 100 nanometers (nm) with specific surface area (SSA) in the 30 – 50 m 2 /g range. Nano Lutetium Particles are also available in passivated and Ultra high purity and high purity and coated and dispersed forms. Research into applications for Lutetium nanocrystals has focused on use as a dopant in glass, laser optics and optical fibers, in phosphors, nanophosphors and doped phosphorous nanoparticles and for their potential electrical, dielectric, magnetic, optical, imaging, catalytic, biomedical and bioscience properties and for use in coatings, plastics, nanowire, and in alloy and catalyst applications.
Physical Properties Metric English Comments
Density 9.841 g/cc
0.3555 lb/in³
Particle Size 0.010 - 0.10 µm
0.010 - 0.10 µm
Specific Surface Area 30 - 50 m²/g
30 - 50 m²/g
Molecular Weight 174.97 g/mol
174.97 g/mol
Thermal Properties Metric English Comments
Melting Point 1652 °C
3006 °F
Boiling Point 3402 °C
6156 °F
Descriptive Properties Value Comments
Appearance Black
Stability Fairly stable in air