American Elements Gadolinium Oxide Nanopowder

Category Ceramic , Oxide
Manufacturer American Elements
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF American Elements Gadolinium Oxide Nanopowder.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
General DescriptionGD-MITE powders and dispersions are inorganic gadolinium-oxide nanoparticles. GD-MITE-A products are uncoated and hydrophilic. GD-MITE-O products are coated with an organic silane (1-4%) and are hydrophobic. Particles are available in the size range of 10-200 nm.
Physical Properties Metric English Comments
Density 7.10 g/cc
0.257 lb/in³
Molecular Weight 362.5 g/mol
362.5 g/mol
Thermal Properties Metric English Comments
Melting Point 2420 °C
4390 °F
Descriptive Properties Value Comments
Appearance White
Solubility Insoluble in water, moderately soluble in strong mineral acids
Stability Slightly hygroscopic