American Elements Cerium Nanoparticles

Category Metal , Pure Element
Manufacturer American Elements
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF American Elements Cerium Nanoparticles.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
General DescriptionCerium (Ce) Nanoparticles, nanodots or nanopowder are black spherical high surface area particles. Nanoscale Cerium Particles are typically 5 - 40 nanometers (nm) with specific surface area (SSA) in the 30 – 50 m 2 /g range and also available in with an average particle size of 60 - 100 nm range with a specific surface area of approximately 5 - 10 m 2 /g. Nano Cerium Particles are also available in passivated and Ultra high purity and high purity and coated and dispersed forms. Applications for cerium nanocrystals include numerous fuel cell functions such as in the electrolyte of solid oxide fuel cells (SOFC), to remove ultrafine diesel particle emissions like carbon and in coatings, plastics, nanowire, nanofiber and textiles and in certain alloy and catalyst applications. Further research is being done for their potential electrical, dielectric, magnetic, optical, imaging, catalytic, biomedical and bioscience properties.
Physical Properties Metric English Comments
Density 6.689 g/cc
0.2417 lb/in³
Particle Size 0.0050 - 0.040 µm
0.0050 - 0.040 µm
0.060 - 0.10 µm
0.060 - 0.10 µm
Specific Surface Area 5.0 - 10 m²/g
5.0 - 10 m²/g
30 - 50 m²/g
30 - 50 m²/g
Molecular Weight 140.12 g/mol
140.12 g/mol
Thermal Properties Metric English Comments
Melting Point 795 °C
1460 °F
Boiling Point 3360 °C
6080 °F
Descriptive Properties Value Comments
Appearance Black
Stability Easily oxidized in the air