Material Notes:
General DescriptionCarbon (C) Nanotubes, Single-Walled, Double Walled and Multi-Walled - Are black nano scale cylindrical tubes of graphitic carbon with numerous applications as the stiffest and strongest known fibers and because of their unique electrical properties. They are available in single walled, double walled and multi-walled forms, bundled and unbundled, with tube lengths from 5 to 30 nanometers (nm) and specific surface area (SSA) in the 50 to 500 m 2 /g range. Carbon Nanotubes are available in ultra high purity and high purity and coated suspended and dispersed forms. Applications for Carbon Nanotubes include in flat screen displays, scanning probe microscopes in brushes for commercial electric motors, and in sensing devices and because of their strength in numerous aerospace and automotive uses, in body armor and tear-resistant cloth fibers and textiles and stronger and lighter sports equipment. Carbon nanotubes can behave like a conductive metallic or semiconductor depending on their structure, which is useful for nanoscale electronic devices and in electrically conductive films in coatings, plastics, nanowire, nanofiber and in certain bioscience applications.
Physical Properties Metric English Comments
Specific Surface Area 50 - 500 m²/g
50 - 500 m²/g
Descriptive Properties Value Comments
Appearance Black
Users viewing this material also viewed the following: