Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

American Elements Boron Nitride Nanoparticles

Category Ceramic , Nitride
Manufacturer American Elements
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF American Elements Boron Nitride Nanoparticles.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
General DescriptionBoron Nitride (BN) Nanoparticles, nanodots or nanopowder are spherical high surface area particles. Nanoscale Boron Nitride Particles are typically 10 - 100 nanometers (nm) with specific surface area (SSA) in the 10 – 75 m 2 /g range. Nano Boron Nitride Particles are also available in Ultra high purity and high purity and coated and dispersed forms. Research into applications for Boron Nitride nanocrystals include use in coatings and microcoatings for precision cutting tools to vary the properties depending on the desired abrasive, lubricating, anti-corrosion, super-hydrophobic, and thermal functions and for use in other aerospace coatings, in particular, as thermal and oxidative protection for fiber reinforced construction materials, such as coating carbon fiber materials with boron nitride, and in plastics, and other cutting applications. Further application could arise in sensor technology, optoelectronics and for space structures.
Physical Properties Metric English Comments
Particle Size 0.010 - 0.10 µm
0.010 - 0.10 µm
Specific Surface Area 10 - 75 m²/g
10 - 75 m²/g
Molecular Weight 24.82 g/mol
24.82 g/mol
Descriptive Properties Value Comments
Appearance White Powder
Users viewing this material also viewed the following: