Material Notes:
Features:nucleationanti-statlow viscosityexcellent processabilityexcellent stiffnessminimal odor or tasteApplications:thin wall partsclosuressmall appliancesFormer A-Top Polymers product; part of Amco product line since 2013.
Physical Properties Metric English Comments
Density 0.910 g/cc
0.0329 lb/in³
ASTM D1505
Melt Index of Compound 20 g/10 min

@Temperature 230 °C
20 g/10 min

@Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 40.0 MPa
5800 psi
50 mm/min; ASTM D638
Elongation at Yield 6.5 %
6.5 %
50 mm/min; ASTM D638
Flexural Modulus 1.86 GPa
270 ksi
1.3 mm/min, 1% Secant; ASTM D790
Izod Impact, Notched 0.320 J/cm

@Temperature 22.8 °C
0.600 ft-lb/in

@Temperature 73.0 °F
ASTM D256