Amco PRIMATOP PP HOMO 120 Injection Molding Polypropylene

Category Polymer , Thermoplastic , Polypropylene (PP)
Manufacturer Amco Plastic Materials
Trade Name PRIMATOP
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Amco PRIMATOP PP HOMO 120 Injection Molding Polypropylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Features:medium viscosityexcellent processabilitygood stiffnessenvironmental stress crack resistanceheat performanceminimal odor and tasteApplications:closuressmall applianceshousewarestoyscontains a unique combination of stabilizersFormer A-Top Polymers product; part of Amco product line since 2013.
Physical Properties Metric English Comments
Density 0.906 g/cc
0.0327 lb/in³
ASTM D1505
Melt Index of Compound 12 g/10 min

@Temperature 230 °C
12 g/10 min

@Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 111
111
ASTM D785
Tensile Strength, Yield 37.6 MPa
5450 psi
50 mm/min; ASTM D638
Elongation at Yield 8.0 %
8.0 %
50 mm/min; ASTM D638
Flexural Modulus 1.55 GPa
225 ksi
1.3 mm/min, 1% Secant; ASTM D790
Izod Impact, Notched 0.374 J/cm

@Temperature 22.8 °C
0.700 ft-lb/in

@Temperature 73.0 °F
ASTM D256