Material Notes:
PP HOMO 040 features low water carry over, excellent melt stability, and contains a unique combination of stabilizers. Applications include slit tape fabric stock and cordage.Former A-Top Polymers product; part of Amco product line since 2013.
Physical Properties Metric English Comments
Density 0.903 g/cc
0.0326 lb/in³
ASTM D1505
Melt Index of Compound 4.0 g/10 min

@Temperature 230 °C
4.0 g/10 min

@Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 109
109
ASTM D785
Tensile Strength, Yield 39.3 MPa
5700 psi
50 mm/min; ASTM D638
Elongation at Yield 9.0 %
9.0 %
50 mm/min; ASTM D638
Flexural Modulus 1.52 GPa
220 ksi
1.3 mm/min, 1% Secant; ASTM D790
Izod Impact, Notched 0.374 J/cm

@Temperature 22.8 °C
0.700 ft-lb/in

@Temperature 73.0 °F
ASTM D256