Material Notes:
PP CO 350-40 features impact resistance and low temperature stiffness. Applications include injection molding and containers.Former A-Top Polymers product; part of Amco product line since 2013.
Physical Properties Metric English Comments
Specific Gravity 0.900 g/cc

@Temperature 23.0 °C
0.900 g/cc

@Temperature 73.4 °F
ASTM D792
Melt Index of Compound 35 g/10 min

@Load 2.16 kg,
Temperature 230 °C
35 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 20.7 MPa
3000 psi
2 in/min; ASTM D638
Elongation at Yield 5.0 %
5.0 %
ASTM D638
Flexural Modulus 0.931 GPa
135 ksi
0.05 in/min, 1% Secant; ASTM D790
Izod Impact, Notched 1.92 J/cm

@Temperature 22.8 °C
3.60 ft-lb/in

@Temperature 73.0 °F
Method A; ASTM D256