Material Notes:
PP CO 350-20 has easy mold flow and excellent dimensional stability. It is used in thin walled injection molded applications.Former A-Top Polymers product; part of Amco product line since 2013.
Physical Properties Metric English Comments
Density 0.900 g/cc
0.0325 lb/in³
ASTM D1505
Melt Index of Compound 36 g/10 min

@Temperature 230 °C
36 g/10 min

@Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 104
104
ASTM D785
Tensile Strength, Yield 23.4 MPa
3400 psi
50 mm/min; ASTM D638
Flexural Modulus 1.02 GPa
148 ksi
1% Secant; ASTM D790
Izod Impact, Notched 1.01 J/cm

@Temperature 22.8 °C
1.90 ft-lb/in

@Temperature 73.0 °F
ASTM D256