Amco PRIMATOP LLDPE 009919B Linear Low Density Polyethylene, Butene Copolymer for Film

Category Polymer , Film , Thermoplastic , Polyethylene (PE) , LLDPE , Linear Low Density Polyethylene (LLDPE)/Butene, Film
Manufacturer Amco Plastic Materials
Trade Name PRIMATOP
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Amco PRIMATOP LLDPE 009919B Linear Low Density Polyethylene, Butene Copolymer for Film.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LLDPE 009919B features excellent toughness and strength when drawn down to thin gauges. Applications include blending resin, industrial packaging, coextrusion, industrial liners, and garment bags.Former A-Top Polymers product; part of Amco product line since 2013.
Physical Properties Metric English Comments
Density 0.919 g/cc
0.0332 lb/in³
ASTM D1505
Melt Index of Compound 0.95 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.95 g/10 min

@Load 4.76 lb,
Temperature 374 °F
Condition E; ASTM D1238
Mechanical Properties Metric English Comments
Film Elongation at Break, MD 540 %
540 %
ASTM D746
Film Elongation at Break, TD 800 %
800 %
ASTM D746
Elmendorf Tear Strength, MD 4.33 g/micron
110 g/mil
ASTM D1922
Elmendorf Tear Strength, TD 25.6 g/micron
650 g/mil
ASTM D1922
Dart Drop 2.95 g/micron
75.0 g/mil
ASTM D1790
Film Tensile Strength at Break, MD 31.7 MPa
4600 psi
ASTM D882
Film Tensile Strength at Break, TD 24.1 MPa
3500 psi
ASTM D882
Optical Properties Metric English Comments
Haze 22 %
22 %
ASTM D1003
Gloss 25 %
25 %
45°; ASTM D790