Material Notes:
Amco Amalloy B1017 is a clear performance copolymer with exceptional clarity and toughness.High melt-flow, very clear.Information provided by Amco Plastic Materials.
Physical Properties Metric English Comments
Specific Gravity 1.04 g/cc
1.04 g/cc
ASTM D1505
Melt Flow 7.5 g/10 min

@Load 1.20 kg,
Temperature 300 °C
7.5 g/10 min

@Load 2.65 lb,
Temperature 572 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 23.4 MPa
3400 psi
ASTM D638
Izod Impact, Notched 0.230 J/cm
0.430 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Vicat Softening Point 101 °C
214 °F
ASTM D648
Optical Properties Metric English Comments
Haze 1.8 %

@Thickness 2.54 mm
1.8 %

@Thickness 0.100 in
ASTM D1003
Transmission, Visible 91 %

@Thickness 2.54 mm
91 %

@Thickness 0.100 in
ASTM D1003