Category | Polymer , Thermoplastic , Fluoropolymer |
Manufacturer | AlphaGary |
Trade Name | Smokeguard™ |
Port | Ningbo port,China |
Trade Terms | FOB, CFR, CIF |
Payment Terms | L/C, T/T, Western Union |
Download PDF | AlphaGary Smokeguard™ HP 700 High Performance Fluoropolymer.pdf |
Price | EMAIL US sales@lookpolymers.com |
Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Hardness, Shore D | 59 | 59 | |
Tensile Strength | 14.5 MPa | 2100 psi | |
Elongation at Break | 280 % | 280 % |
Thermal Properties | Metric | English | Comments |
---|---|---|---|
Brittleness Temperature | -52.0 °C | -61.6 °F | |
Oxygen Index | 99 % | 99 % |