AlphaGary Smokeguard™ HP 505 High Performance Fluoropolymer

Category Polymer , Thermoplastic , Fluoropolymer
Manufacturer AlphaGary
Trade Name Smokeguard™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF AlphaGary Smokeguard™ HP 505 High Performance Fluoropolymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Smokeguard™ HP is a high performance fluoropolymer compound with excellent flame and smoke properties intended for difficult constructions and test requirements
Mechanical Properties Metric English Comments
Hardness, Shore D 60
60
Tensile Strength 17.2 MPa
2500 psi
Elongation at Break 400 %
400 %
Thermal Properties Metric English Comments
Brittleness Temperature -13.0 °C
8.60 °F
Oxygen Index 45 %
45 %