AlphaGary PVC GM 8001-E Natural LCF Polyvinyl Chloride Thermoplastic

Category Polymer , Thermoplastic , Vinyl (PVC) , PVC, Molded
Manufacturer AlphaGary
Trade Name PVC
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF AlphaGary PVC GM 8001-E Natural LCF Polyvinyl Chloride Thermoplastic.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
A lead free, flame retarded, V-O rated compound designed for plug molding
Mechanical Properties Metric English Comments
Hardness, Shore A 88 - 95
88 - 95
Tensile Strength 16.5 MPa
2400 psi
Elongation at Break 250 %
250 %
ASTM D412
Thermal Properties Metric English Comments
Brittleness Temperature -20.0 °C
-4.00 °F
Flammability, UL94 V-0
V-0
Oxygen Index 30 %
30 %