AlphaGary PVC 2228C/FS-65S WHITE 4001 Polyvinyl Chloride Thermoplastic

Category Polymer , Thermoplastic , Vinyl (PVC) , PVC, Extruded
Manufacturer AlphaGary
Trade Name PVC
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF AlphaGary PVC 2228C/FS-65S WHITE 4001 Polyvinyl Chloride Thermoplastic.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Self-frosting, low coefficient of frictionFormulated for extrusion
Mechanical Properties Metric English Comments
Hardness, Shore A 65
65
Descriptive Properties Value Comments
DEHP Free No
Phthalate Free Yes