AlphaGary Garathane™ X 96-320 B Polyurethane based compound

Category Polymer , Thermoplastic , Polyurethane, TP
Manufacturer AlphaGary
Trade Name Garathane™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF AlphaGary Garathane™ X 96-320 B Polyurethane based compound.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
For Boots
Physical Properties Metric English Comments
Specific Gravity 1.23 g/cc
1.23 g/cc
Mechanical Properties Metric English Comments
Hardness, Shore A 54 - 62
54 - 62
Tensile Strength 9.38 MPa
1360 psi
Elongation at Break 370 %
370 %
Flex Crack Resistance 20000
20000
Ross Flex