AlphaGary Garathane™ X 94-350-B UV-DG2 Polyurethane based compound

Category Polymer , Thermoplastic , Polyurethane, TP
Manufacturer AlphaGary
Trade Name Garathane™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF AlphaGary Garathane™ X 94-350-B UV-DG2 Polyurethane based compound.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
90°C rated flame retardant, polyether based, polyurethane compound
Mechanical Properties Metric English Comments
Hardness, Shore A 82 - 87
82 - 87
Tensile Strength 11.0 MPa
1600 psi
Elongation at Break 600 %
600 %
ASTM D412
Thermal Properties Metric English Comments
Oxygen Index 30 %
30 %