AlphaGary Garaflex™ X 97-234 D Vinyl Thermoplastic Elastomer

Category Polymer , Thermoplastic , Elastomer, TPE , Vinyl (PVC)
Manufacturer AlphaGary
Trade Name Garaflex™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF AlphaGary Garaflex™ X 97-234 D Vinyl Thermoplastic Elastomer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Garaflex™ is a vinyl based thermoplastic elastomer used mostly in footwearOil & Fuel Resistant
Physical Properties Metric English Comments
Specific Gravity 1.21 g/cc
1.21 g/cc
Mechanical Properties Metric English Comments
Hardness, Shore A 55 - 65
55 - 65
Flex Crack Resistance 20000
20000
Ross Flex