Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

AlphaGary Garaflex™ E 4762-A5 LCF Vinyl Thermoplastic Elastomer

Category Polymer , Thermoplastic , Elastomer, TPE , Vinyl (PVC) , PVC, Wire and Cable Grade
Manufacturer AlphaGary
Trade Name Garaflex™ E
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF AlphaGary Garaflex™ E 4762-A5 LCF Vinyl Thermoplastic Elastomer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Garaflex™ E is a vinyl based thermoplastic elastomer used mostly in wire and cable105°C rated flexible jacket / insulation compound with excellent low temperature properties
Mechanical Properties Metric English Comments
Hardness, Shore A 65 - 74
65 - 74
Tensile Strength 13.8 MPa
2000 psi
Elongation at Break 300 %
300 %
ASTM D412
Thermal Properties Metric English Comments
Brittleness Temperature -53.0 °C
-63.4 °F
Oxygen Index 24 %
24 %