Material Notes:
Zythane™ 4065D is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good hydrolytic stability, oil, fuel and solvent resistance. It is supplied uncolored in pellet form. Availability: North AmericaFeatures: Fuel Resistant, Good Toughness, Oil Resistant, Hydrolytically Stable, Solvent Resistant, Good Abrasion Resistance Appearance: ColorlessForms: PelletsProcessing Method: Injection MoldingInformation provided by Alliance Polymers
Physical Properties Metric English Comments
Density 1.23 g/cc
0.0444 lb/in³
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore D 64
64
ASTM D2240
Tensile Strength at Break 55.0 MPa
7980 psi
ASTM D412
Tensile Stress 20.0 MPa

@Strain 100 %
2900 psi

@Strain 100 %
ASTM D412
40.0 MPa

@Strain 300 %
5800 psi

@Strain 300 %
ASTM D412
Elongation at Break 340 %
340 %
ASTM D412
Tear Strength 140 kN/m
799 pli
Die C; ASTM D412
Taber Abrasion, mg/1000 Cycles 45
45
ASTM D1044
Abrasion 50
50
mm<sup>3</sup>; DIN 53516
Compression Set 38 %

@Temperature 22.8 °C,
Time 79200 sec
38 %

@Temperature 73.0 °F,
Time 22.0 hour
ASTM D3995B
48 %

@Temperature 70.0 °C,
Time 259000 sec
48 %

@Temperature 158 °F,
Time 72.0 hour
ASTM D3995B
Thermal Properties Metric English Comments
Vicat Softening Point 152 °C
306 °F
ASTM D1525
Brittleness Temperature -5.00 °C
23.0 °F
ASTM D746
Flammability, UL94 HB

@Thickness 1.00 mm
HB

@Thickness 0.0394 in
HB

@Thickness 1.50 mm
HB

@Thickness 0.0591 in
HB

@Thickness 3.00 mm
HB

@Thickness 0.118 in
Processing Properties Metric English Comments
Processing Temperature 220 - 230 °C
428 - 446 °F
Injection
Rear Barrel Temperature 205 °C
401 °F
Injection
Middle Barrel Temperature 215 °C
419 °F
Injection
Front Barrel Temperature 225 °C
437 °F
Injection
Nozzle Temperature 220 - 230 °C
428 - 446 °F
Injection
Mold Temperature 25.0 - 60.0 °C
77.0 - 140 °F
Injection
Injection Velocity >= 10.0 mm/sec
>= 0.394 in/sec
Injection
Drying Temperature 90.0 °C
194 °F
Injection
Dry Time 4.00 hour
4.00 hour
Injection
Back Pressure 0.600 - 1.40 MPa
87.0 - 203 psi
Injection
Clamp Pressure 49.6 - 89.6 MPa
7200 - 13000 psi
Injection
Screw Speed 60 - 200 rpm
60 - 200 rpm
Injection