Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Alcoa KAMA 5100 CPET  (discontinued **)

Category Polymer , Thermoplastic , Polyester, TP , Polyethylene Terephthalate (PET)
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Alcoa KAMA 5100 CPET  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
CapabilitiesGauge: .020" to .040" (508 to 106µm)Width: 20" to 52" (508 to 1321mm)Core size: 3" or 6"Roll O.D.: 29" standard, available up to 40"Silicone coating availableAvailable in natural blackPropertiesExcellent for dual-ovenable applicationsGood impact performanceIdeal for home meal replacement applicationsFDA compliant to CFR 21 #177.1630Kosher materialInformation provided by Alcoa Kama Co.
Physical Properties Metric English Comments
Specific Gravity 1.33 g/cc
1.33 g/cc
Viscosity Measurement 0.78 - 0.85
0.78 - 0.85
Intrinsic Viscosity; ASTM D3835
Thickness 508 - 1020 microns
20.0 - 40.0 mil
Linear Mold Shrinkage 0.010 - 0.018 cm/cm
0.010 - 0.018 in/in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength, Yield 34.5 - 62.1 MPa
5000 - 9000 psi
ASTM D638
Elongation at Break 100 - 400 %
100 - 400 %
ASTM D638
Flexural Modulus 2.07 - 2.76 GPa
300 - 400 ksi
ASTM D790
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 177 °C
350 °F
Minimum Service Temperature, Air -12.2 °C
10.0 °F
Processing Properties Metric English Comments
Processing Temperature 138 - 160 °C
280 - 320 °F
Thermoforming Temp
Descriptive Properties Value Comments
Resistance to Acid Good to Excellent
Resistance to Alcohols Good to Excellent
Resistance to Alkalis Fair to Good
Resistance to Fat, Grease, and Oil Good to Excellent
Resistance to Hydrocarbon Solvents Good to Excellent
Resistance to Strong Oxidizers Good to Excellent
Yield, in²/lb/mil 20810
Copyright © lookpolymers.com All Rights Reserved