Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Alcoa KAMA 4100 Prime APET  (discontinued **)

Category Polymer , Thermoplastic , Polyester, TP , Polyethylene Terephthalate (PET)
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Alcoa KAMA 4100 Prime APET  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
CapabilitiesGauge: .007” to .050” (178 to 1270µm)Width: 12” to 48” (305 to 1219mm)Core size: 6” standard, 3” and 8” availableRoll O.D.: 29” standard, available up to 40”Available in clear, colored and tintedGraphic arts availableSilicone coating availableMedical grade material available4 strategic manufacturing locationsPropertiesExceptional clarity and impact performanceGood formability with great definitionFaster forming cycles than PVCExcellent strength for tough POP applications100% recyclableFDA accepted materialKosher materialFDA compliant to CFR 21 #177.1630Information provided by Alcoa Kama Co.
Physical Properties Metric English Comments
Specific Gravity 1.33 g/cc
1.33 g/cc
Viscosity Measurement >= 0.74
>= 0.74
Intrinsic Viscosity; ASTM D3835
Thickness 178 - 1270 microns
7.00 - 50.0 mil
Linear Mold Shrinkage 0.020 - 0.050 cm/cm
0.020 - 0.050 in/in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength, Yield 55.2 - 62.1 MPa
8000 - 9000 psi
ASTM D638
Elongation at Break 200 - 400 %
200 - 400 %
ASTM D638
Flexural Modulus 2.24 - 2.55 GPa
325 - 370 ksi
ASTM D790
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 65.6 °C
150 °F
Minimum Service Temperature, Air -17.8 °C
0.000 °F
Optical Properties Metric English Comments
Haze <= 2.0 %
<= 2.0 %
ASTM D1003
Transmission, Visible >= 90 %
>= 90 %
ASTM D1003
Processing Properties Metric English Comments
Processing Temperature 121 - 154 °C
250 - 310 °F
Thermoforming Temp
Descriptive Properties Value Comments
Clarity, % >99
Resistance to Acid Good to Excellent
Resistance to Alcohols Good to Excellent
Resistance to Alkalis Fair to Good
Resistance to Fat, Grease, and Oil Good to Excellent
Resistance to Hydrocarbon Solvents Good to Excellent
Resistance to Strong Oxidizers Good to Excellent
Yield, in²/lb/mil 20810