Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Alcoa KAMA 2600 Envelope Window, Film  (discontinued **)

Category Polymer , Film , Thermoplastic , Polystyrene (PS)
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Alcoa KAMA 2600 Envelope Window, Film  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
CapabilitiesGauge: .001” to .004” (28 to 101µm)Width: .2” to 80” (50.8 to 2032mm)Core size: 3” and 6” standard cores, 8” availableRoll O.D.: various confiations availableCustom colors and tints available3 strategic manufacturing locationsPropertiesLow gloss formula for better optical character recognitionLow dust for higher production ratesEngineered orientation for optimal tear propertiesSpecially formulated to reduce scratchingExcellent stiffness for improved processabilityInformation provided by Alcoa Kama Co.
Physical Properties Metric English Comments
Specific Gravity 1.05 g/cc
1.05 g/cc
Thickness 25.4 - 50.8 microns
1.00 - 2.00 mil
Mechanical Properties Metric English Comments
Tensile Strength, Yield 55.2 - 82.7 MPa
8000 - 12000 psi
ASTM D638
Elongation at Break 3.0 - 10 %
3.0 - 10 %
ASTM D638
Tensile Modulus 2.76 - 3.10 GPa
400 - 450 ksi
ASTM D790
Descriptive Properties Value Comments
Resistance to Acid Good to Excellent
Resistance to Alcohols Good to Excellent
Resistance to Alkalis Excellent
Resistance to Fat, Grease, and Oil Good
Resistance to Hydrocarbon Solvents Poor
Resistance to Strong Oxidizers Poor
Yield, in²/lb/mil 26360
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved