Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Albis Plastics Tedur® L V 9404-1 PPS, 30% Carbon Fiber  (discontinued **)

Category Polymer , Thermoplastic , Polyphenylene Sulfide (PPS) , Polyphenylene Sulfide (PPS) with 30% Carbon Fiber Filler
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Albis Plastics Tedur® L V 9404-1 PPS, 30% Carbon Fiber  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
High Electrical and Thermal Conductivity, Long-term Anti-static Properties. Incandescent wire resistance (2 mm) is 960°C per VDE 0471 T1.2.Applications: Fan Blades, Brake Sleeves, Model Construction Rotor BladesProcessing: Injection Molding (Melt Temperature: 610-645°F, Mold Temperature: 285°F)Tedur® is manufactured by Albis Plastics Corporation under license of the registered trademark owner (Bayer.) Data supplied by Albis Plastics Corporation.
Physical Properties Metric English Comments
Density 1.45 g/cc
0.0524 lb/in³
DIN 53 47
Mechanical Properties Metric English Comments
Elongation at Break 2.5 %
2.5 %
DIN 53 455
Flexural Yield Strength 280 MPa
40600 psi
DIN 53 452
Flexural Modulus 23.0 GPa
3340 ksi
DIN 53 457
Compressive Yield Strength 190 MPa
27600 psi
ASTM D695
Izod Impact, Notched 2.51 J/cm
4.70 ft-lb/in
Approximation; ISO 180/1U
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 260 °C
500 °F
ASTM D648
Flammability, UL94 V-0
V-0
Albis North America Internal Test
Electrical Properties Metric English Comments
Surface Resistance <= 100 ohm
<= 100 ohm
DIN 53 482
Processing Properties Metric English Comments
Melt Temperature 321 - 341 °C
610 - 646 °F
Injection
Mold Temperature 141 °C
286 °F
Users viewing this material also viewed the following: