Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Albis Plastics Tedur® L 9560 PPS, 50% Mineral

Category Polymer , Thermoplastic , Polyphenylene Sulfide (PPS)
Manufacturer Albis Plastics
Trade Name Tedur®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Albis Plastics Tedur® L 9560 PPS, 50% Mineral.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
High Gloss, Highest Surface Finish, Metallization w/o Base Coating. Incandescent wire resistance (2 mm) is 960°C per VDE 0471 T1.2.Applications: Various High Temperature ReflectorsProcessing: Injection Molding (Melt Temperature: 610-645°F, Mold Temperature: 285°F)Tedur® is manufactured by Albis Plastics Corporation under license of the registered trademark owner (Bayer.) Data supplied by Albis Plastics Corporation.
Physical Properties Metric English Comments
Density 1.82 g/cc
0.0658 lb/in³
DIN 53 47
Mechanical Properties Metric English Comments
Tensile Strength at Break 50.0 MPa
7250 psi
DIN 53 455
Elongation at Break 0.50 %
0.50 %
DIN 53 455
Modulus of Elasticity 7.80 GPa
1130 ksi
DIN 53 457
Flexural Yield Strength 75.0 MPa
10900 psi
DIN 53 452
Flexural Modulus 13.0 GPa
1890 ksi
DIN 53 457
Izod Impact, Notched 1.17 J/cm
2.19 ft-lb/in
Approximation; ISO 180/1U
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 196 °C
385 °F
ASTM D648
Flammability, UL94 V-0
V-0
Electrical Properties Metric English Comments
Comparative Tracking Index 175 V
175 V
IEC 112
Processing Properties Metric English Comments
Melt Temperature 321 - 341 °C
610 - 646 °F
Injection
Mold Temperature 141 °C
286 °F
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved