Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Albis Plastics Tedur® L 9510-1 PPS, 40% Glass Fiber

Category Polymer , Thermoplastic , Polyphenylene Sulfide (PPS) , Polyphenylene Sulfide (PPS) with 40% Glass Fiber Filler
Manufacturer Albis Plastics
Trade Name Tedur®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Albis Plastics Tedur® L 9510-1 PPS, 40% Glass Fiber.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
High Strength, High Rigidity Standard Grade. Incandescent wire resistance (2 mm) is 960°C per VDE 0471 T1.2.Applications: Pump Impellers, Valve Housings and BushingsProcessing: Injection Molding (Melt Temperature: 610-645°F, Mold Temperature: 285°F)Tedur® is manufactured by Albis Plastics Corporation under license of the registered trademark owner (Bayer.) Data supplied by Albis Plastics Corporation.
Physical Properties Metric English Comments
Density 1.65 g/cc
0.0596 lb/in³
DIN 53 47
Mechanical Properties Metric English Comments
Tensile Strength at Break 185 MPa
26800 psi
DIN 53 455
Elongation at Break 1.7 %
1.7 %
DIN 53 455
Modulus of Elasticity 14.5 GPa
2100 ksi
DIN 53 457
Flexural Yield Strength 260 MPa
37700 psi
DIN 53 452
Flexural Modulus 13.0 GPa
1890 ksi
DIN 53 457
Izod Impact, Notched 3.52 J/cm
6.59 ft-lb/in
Approximation; ISO 180/1U
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 260 °C
500 °F
ASTM D648
Flammability, UL94 V-0
V-0
Processing Properties Metric English Comments
Melt Temperature 321 - 341 °C
610 - 646 °F
Injection
Mold Temperature 141 °C
286 °F
Copyright © lookpolymers.com All Rights Reserved