Category Polymer , Thermoplastic , Nylon , Nylon 6/66 , Nylon 66/6, 30% Glass Fiber Reinforced
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Albis Plastics Polyamide 6/66 PA 152 GF30/02 BK8-1114 Black 30% Glass Fiber  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Semi-crystalline Nylon 6/66 (PA6/66)Characteristics: Industrial GradeApplications: Office Furniture, Gear, Housings and ConnectorsProcessing: Injection Molding (Melt Temperature: 465 -555°F, Mold Temperature: 175-230°F)Data supplied by Albis Plastics Corporation.
Physical Properties Metric English Comments
Density 1.36 g/cc
0.0491 lb/in³
ASTM D792
Linear Mold Shrinkage 0.0020 - 0.0040 cm/cm
0.0020 - 0.0040 in/in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength, Yield 141.3 MPa
20490 psi
ASTM D638
Elongation at Break 2.67 %
2.67 %
ASTM D638
Flexural Yield Strength 211.2 MPa
30630 psi
ASTM D790
Flexural Modulus 8.10 GPa
1170 ksi
ASTM D790
Izod Impact, Notched 0.720 J/cm
1.35 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 249 °C
480 °F
ASTM D648
Flammability, UL94 HB
HB
0.125 in; Albis Internal Test
Processing Properties Metric English Comments
Melt Temperature 241 - 291 °C
466 - 556 °F
Injection
Mold Temperature 79.0 - 110 °C
174 - 230 °F