Albis Plastics Cellulose Acetate Butyrate B9424-3 , 3% Plasticizer  (discontinued **)

Category Polymer , Renewable/Recycled Polymer , Thermoplastic , Cellulosic , Cellulose Acetate Butyrate, Molded
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Albis Plastics Cellulose Acetate Butyrate B9424-3 , 3% Plasticizer  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Amorphous Cellulose Acetate Butyrate (CAB)Characteristics: Dimensional Stability, Weatherability and Low Temp Impact StrengthApplications: Pens, Ski Goggles, Auto Trim, Skylights, Tool Handles and ToysProcessing: Injection Molding (Melt Temperature: 475°F, Mold Temperature: 175°F)Data supplied by Albis Plastics Corporation.
Physical Properties Metric English Comments
Density 1.21 g/cc
0.0437 lb/in³
ASTM D792
Water Absorption 1.8 %
1.8 %
(24 hr); ASTM D570
Mechanical Properties Metric English Comments
Tensile Strength at Break 52.4 MPa
7600 psi
ASTM D638
Tensile Strength, Yield 44.5 MPa
6450 psi
ASTM D638
Elongation at Break 50 %
50 %
ASTM D638
Izod Impact, Notched 1.44 J/cm
2.70 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 86.0 °C
187 °F
ASTM D648
Vicat Softening Point 118 °C
244 °F
ASTM D1525
Processing Properties Metric English Comments
Melt Temperature 246 °C
475 °F
Injection
Mold Temperature 79.0 °C
174 °F