Akzo Nobel Trigonox® ESP Peroxide Cure Agent

Category Other Engineering Material , Catalyst/Initiator , Polymer
Manufacturer Akzo Nobel
Trade Name Trigonox®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Akzo Nobel Trigonox® ESP Peroxide Cure Agent.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Trigonox ESP is a peroxide formulation for the curing of unsaturated polyester resins in the presence of a cobalt accelerator.Chemical Description: Methyl isobutyl ketone peroxide and cyclohexanone peroxide, 38% in solvent mixtureCAS Number: 37206-20-5; 12262-58-7Acronym: MIBKP; COX; Tx ESPInformation provided by Akzo Nobel Polymer Chemicals.
Physical Properties Metric English Comments
Storage Temperature <= 25.0 °C
<= 77.0 °F