Akzo Nobel Trigonox® EHPS Polymerization Initiator

Category Other Engineering Material , Catalyst/Initiator , Polymer
Manufacturer Akzo Nobel
Trade Name Trigonox®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Akzo Nobel Trigonox® EHPS Polymerization Initiator.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Initiator for the (co)polymerization of styrene, acrylonitrile, vinylacetate, vinylchloride, vinylidenechloride, acrylates and methacrylates.Chemical Description: Di(2-ethylhexyl) peroxydicarbonate, with stabilizerCAS Number: 16111-62-9Acronym: EHP; OPP; Tx EHPInformation provided by Akzo Nobel Polymer Chemicals.
Physical Properties Metric English Comments
One Hour Half Life Temperature 64.0 °C
147 °F
Storage Temperature <= -20.0 °C
<= -4.00 °F