Material Notes:
Initiator for the (co)polymerization of ethylene, styrene, acrylates and methacrylates. Trigonox B is a monofunctional peroxide which is used for the crosslinking of polyolefins as well as natural rubber and synthetic rubbers.Chemical Description: Di-tert-butyl peroxideCAS Number: 110-05-4Acronym: DTBP; Tx BInformation provided by Akzo Nobel Polymer Chemicals.
Physical Properties Metric English Comments
One Hour Half Life Temperature 141 °C
286 °F
Storage Temperature -30.0 - 40.0 °C
-22.0 - 104 °F