Material Notes:
The product types are mainly used in the automobile industry sector, but also for the domestic industry, the building industry and the leisure time-and sporting goods industry, AKROMID has become a considerable factor.Information from Akro-Plastic
Mechanical Properties Metric English Comments
Tensile Stress 120 MPa
17400 psi
Charpy Impact, Notched 1.20 J/cm²
5.71 ft-lb/in²